Concrete strength and shrinkage reducer
If you are looking for high-quality products, please feel free to contact us and send an inquiry, email: brad@ihpa.net
The purchasing pace at the demand end of the international thermal coal market continues to slow down and the international thermal coal price continues to decline. Prices for thermal coal at major international ports continued to fall last week as buyers in Europe slowed in recent days for April, coupled with weaker-than-expected import demand from End users in China. According to China Coal Market net monitoring: Australia Newcastle port thermal coal price index was 253 USD/ton, compared with 309.02 USD/ton, down 56.02 USD/ton, down 18.13%. South Africa's Port Richards thermal coal price Index was $264.5 / mt, down the US $62.72 / mt or 19.17% from US $327.22 / mt. The European ARA Tri-port thermal coal price Index was $281.8 / ton. Does the price of thermal coal in major international ports continue to decline to affect the price of the Concrete strength and shrinkage reducer?
Description of Concrete strength and shrinkage reducer
1. After adding concrete strength shrinkage enhancer to carbonate cement, it can effectively improve the early and late strength (strength is increased by 5-30%), improve the mold turnover rate, and can also reduce the steam curing temperature or shorten the steam curing time.
2. The coagulant strength-promoting and shrinkage-reducing agent gives the micro-expansion performance to compensate for dry shrinkage, reduce the mixing shrinkage, and improve the crack resistance.
3. Adding a strength-promoting shrink-reducing agent can greatly reduce the amount of Portland cement and reduce the cost of concrete when the early strong friction is not pursued.
4. The dosage of Portland cement can be appropriately reduced after adding concrete strength-enhancing and shrinkage-reducing agent, and low cement and low glue material can still be prepared to reduce the hydration heat release of high-grade and large-volume concrete, and reduce the temperature difference between the center temperature and the surface temperature of the concrete. Reduce the risk of cracking in mass concrete.
5. The strength, impermeability, freeze-thaw resistance, carbonization resistance, and volumetric properties of concrete mixed with strength-promoting shrinkage-reducing agent have been significantly improved.
Indicators of Concrete strength and shrinkage reducer
Items | Required indicators | Test results |
specific surface area | m2/kg | ≥500 | 525 |
Setting time | Initial setting | min | ≥8 | 45 |
Final setting | ≤30 | 20 |
Free expansion rate in water | 7d | ≥0.05 | 0.095 |
Flexural strength | 8h | ≥6.0 | 7.5 |
1d | ≥7.0 | 8.5 |
7d | ≥8.0 | 9.9 |
Compressive strength | 8h | ≥30.0 | 33.0 |
1d | ≥45.0 | 49.9 |
7d | ≥60.0 | 63.6 |
Remark | According to the ingredients of different manufacturers, it needs to be adjusted |
The mechanism of Concrete strength and shrinkage reducer
1. With the addition of strength-promoting and shrinkage-reducing agent, calcium sulfoaluminate minerals, calcium sulfate calcined at a higher temperature, high-activity calcium oxide, and Portland cement are compounded and reacted with water to make the calcium aluminate in Portland cement. The aluminum oxide and calcium oxide in the mixed materials such as minerals and slag react to form ettringite hydrated minerals with fast hardness, high strength and slight swelling, so that the potential activity of the mixed materials such as slag can be fully developed. , thereby improving the early and late strength of concrete.
2. The expansive hydration products such as mayvandite and calcium sulfate in the composite system and the organic and inorganic strength-shrinking-promoting components in the strength-promoting and shrinking-reducing agent have the expansion function to compensate for dry shrinkage and improve the crack resistance of concrete. Densification performance and frost resistance, etc.
3. In the composite system concrete, the cohesion is increased due to physical and chemical effects, and segregation and bleeding are avoided.
4. The alkali-free chemical activator accelerates and improves the degree of hydration of cement minerals, thereby improving the early and early strength of concrete.
5. Expansive hydrates such as ettringite and calcium sulfate in the composite system and the shrinkage-reducing components in the strength-promoting shrinkage-reducing agent improve the crack resistance, compactness, frost resistance and impermeability of the mixed soil.
Suggested addition amount of Concrete strength and shrinkage reducer
5-20% of cement material.
Packaging and storage of Concrete strength and shrinkage reducer
25kg/bag or ton bag
If you want to know more about concrete strength and shrinkage reducer,please feel free and contact us :sales@cabr-concrete.com
Due to the limited total amount of traditional energy, people have a huge demand for cleaner and greener new energy alternatives. Now, the emergence of graphene is unlocking the possibility of its application in the energy field, which can create a greener, more efficient, and sustainable future. Here Francesco Bonaccorso, Deputy Director of Innovation at the Graphene Flagship Program, explains how his researchers have developed a series of initiatives to bring graphene from the lab to the commercial market. Graphene has become a research hotspot for new materials in the 21st century. Graphene has been adopted by many industries, the most notable of which are healthcare and key material applications.
The development of graphene has brought huge fluctuations in the demand for Concrete strength and shrinkage reducer, and the demand for Concrete strength and shrinkage reducer will continue to grow in the future. You can contact us for the latest news on Concrete strength and shrinkage reducer.
Inquiry us